Material Notes:
BETAFOAM™ 87100/87156 is a rigid, all-water blown molded foam with excellent thermal stability. Foam is produced by rapidly mixing both components under high shear conditions. These components were formulated to produce large, highly contoured, thin parts.Information provided by Dow
Physical Properties Metric English Comments
Density 0.0800 g/cc
0.00289 lb/in³
Free Rise Density (Cured)
Water Absorption 2.5 %
2.5 %
SAE J315
Mechanical Properties Metric English Comments
Compressive Strength 0.586 MPa
85.0 psi
10% Deflection; ASTM 1621A
Thermal Properties Metric English Comments
Shrinkage 1.00 %

@Temperature 37.8 °C,
Time 605000 sec
1.00 %

@Temperature 100 °F,
Time 168 hour
95% RH
2.00 %

@Temperature 121 °C,
Time 173000 sec
2.00 %

@Temperature 250 °F,
Time 48.0 hour
3.00 %

@Temperature 80.6 °C,
Time 1800 sec
3.00 %

@Temperature 177 °F,
Time 0.500 hour
Processing Properties Metric English Comments
Gel Time 1.41 - 1.58 min
1.41 - 1.58 min
Descriptive Properties Value Comments
Aged Weight Loss % 3
7days @ 215°F
Volume Expansion %, min 1300
Cured