Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow BETAFOAM™ 87100/87120

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Dow Chemical
Trade Name BETAFOAM™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAFOAM™ 87100/87120.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BETAFOAM™ 87100/87120 is a low density, all water blown rigid polyurethane foam. These components were engineered to produce a foam for providing barrier protection against airborne noise. Foam is produced by the rapid mixing of both components under high shear conditions. These components were formulated for fast reaction and high volume expansion. The foam has adhesion to primed metal surfaces.Information provided by Dow
Physical Properties Metric English Comments
Density 0.0330 g/cc
0.00119 lb/in³
Free Rise Density (Cured)
Water Absorption 6.0 %
6.0 %
Mechanical Properties Metric English Comments
Compressive Strength >= 0.103 MPa
>= 15.0 psi
Thermal Properties Metric English Comments
Shrinkage <= 1.00 %

@Temperature 121 °C,
Time 173000 sec
<= 1.00 %

@Temperature 250 °F,
Time 48.0 hour
<= 1.00 %

@Temperature 37.8 °C,
Time 605000 sec
<= 1.00 %

@Temperature 100 °F,
Time 168 hour
<= 1.00 %

@Temperature 102 °C,
Time 605000 sec
<= 1.00 %

@Temperature 215 °F,
Time 168 hour
Processing Properties Metric English Comments
Gel Time 0.0500 - 0.0670 min
0.0500 - 0.0670 min
Descriptive Properties Value Comments
Aged Weight Loss %, max 1
7days @ 215°F
Volume Expansion %, min 3200
Cured
Users viewing this material also viewed the following: