Dow ATTANE™ 4213 Ultra Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Very Low Density Polyethylene (VLDPE)
Manufacturer Dow Chemical
Trade Name ATTANE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow ATTANE™ 4213 Ultra Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATTANE® 4213 copolymer is an ultra low density polyethylene that offers excellent flexibility, sealability, puncture resistance and superior strength. It exhibits oxygen transmission characteristics that is well suited for produce packaging applications. It complies with FDA regulation 21 CFR 177.1520 c 3.1b.Film properties below based on a film thickness of 51 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
Moisture Vapor Transmission 0.0714 cc-mm/m²-24hr-atm
0.181 cc-mil/100 in²-24hr-atm
or 1.4 g/m²/atm/24 hr
Thickness 51.0 microns
2.01 mil
Melt Flow 0.80 g/10 min

@Load 2.16 kg
0.80 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.7.
Mechanical Properties Metric English Comments
Coefficient of Friction 0.53
0.53
Elmendorf Tear Strength MD 701 g
701 g
Elmendorf Tear Strength TD 1030 g
1030 g
Elmendorf Tear Strength, MD 13.7 g/micron
348 g/mil
Elmendorf Tear Strength, TD 20.2 g/micron
513 g/mil
Dart Drop >= 16.3 g/micron
>= 414 g/mil
Thermal Properties Metric English Comments
Vicat Softening Point 81.0 °C
178 °F
Optical Properties Metric English Comments
Haze 5.5 %
5.5 %
Processing Properties Metric English Comments
Processing Temperature 86.0 °C
187 °F
Seal initiation temperature
228 °C
442 °F
Film extrusion temperature