Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow ATTANE™ 4206 Ultra Low Density Polyethylene, Impact Modifier Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Very Low Density Polyethylene (VLDPE)
Manufacturer Dow Chemical
Trade Name ATTANE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow ATTANE™ 4206 Ultra Low Density Polyethylene, Impact Modifier Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATTANE® 4206 copolymer is an ultra low density polyethylene that offers excellent performance as an impact modifier for durable molded parts. It provides excellent impact and rigidity improvements when blended with polyethylene or polypropylene for use in applications such as pallets, cases, and crates. It complies with FDA regulation 21 CFR 177.1520 c 3.1b.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
Melt Flow 5.0 g/10 min

@Load 2.16 kg
5.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 68.3 MPa
9910 psi
Film Tensile Strength at Yield, TD 66.9 MPa
9700 psi
Film Elongation at Break, MD 605 %
605 %
Film Elongation at Break, TD 866 %
866 %
Elmendorf Tear Strength MD 296 g
296 g
Unspecified film thickness
Elmendorf Tear Strength TD 635 g
635 g
Unspecified film thickness
Dart Drop Test 185 g
0.408 lb
Film Tensile Strength at Break, MD 51.8 MPa
7510 psi
Film Tensile Strength at Break, TD 37.4 MPa
5420 psi
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
Optical Properties Metric English Comments
Haze 0.60 %
0.60 %
Gloss 93 %
93 %