Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer

Category Polymer , Thermoplastic
Manufacturer Dow Chemical
Trade Name AMPLIFY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance toughness of the structure. This product is a low gel MAH-grafted elastomer useful to improve impact resistance for polyamide or other engineering resins and to enhance interlayer adhesion in co-extruded films.Information provided by Dow
Physical Properties Metric English Comments
Density 0.8985 g/cc
0.03246 lb/in³
ASTM D792
Filler Content 0.25 - 0.50 %
0.25 - 0.50 %
MAH graft; Dow Method
Melt Flow 3.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
5 sec; ASTM D2240
91
91
1 sec; ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 0.103 GPa
15.0 ksi
2% Secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 117 °C
243 °F
Dow Method
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
Dow Method