Dow AFFINITY™ EG 8200 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ EG 8200 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® EG 8200 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation. It exhibits excellent flow properties, exceptional heat aging and compression set when crosslinked, excellent weatherability. It is also effective in binder dispersions and as an impact modifier in polyolefins, exhibiting superior impact properties in blends with PE and PP.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Ratio I10/I2 = 7.1
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Tensile Strength at Break 7.60 MPa
1100 psi
Tensile stress at break.
Elongation at Break >= 1000 %
>= 1000 %
100% Modulus 0.00280 GPa
0.406 ksi
Secant Modulus 0.0200 GPa
2.90 ksi
2% Secant Modulus
Tensile Set 0.00 %
0.00 %
Elongation set after break