Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow 6D83K Polypropylene Random Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Blow Molding Grade , Polypropylene, Extrusion Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 6D83K Polypropylene Random Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewConsistent processabilityLow odor and taste transferHigh glossGood regrind stabilityContains clarifying additiveComplies with: U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW 6D83K Polypropylene Resin is intended for use in extrusion blow molding processes where enhanced clarity is desired.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1070 MPa
155000 psi
ASTM D790A
Izod Impact, Notched 2.94 J/cm
5.51 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved