Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow 6D43 Polypropylene Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 6D43 Polypropylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW 6D43 is intended for use fiber spinning processes.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Temperature 230 °C
35 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 10 %
10 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648
Copyright © lookpolymers.com All Rights Reserved