Dow 5D49 Polypropylene Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 5D49 Polypropylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW 5D49 is intended for use fiber spinning processes. It is well suited for spunbond non-woven applications.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 38 g/10 min

@Temperature 230 °C
38 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 7.0 %
7.0 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648