Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dielectric Polymers NT-5521-2 Photo Processing Tape  (discontinued **)

Category Polymer , Adhesive , Tape , Thermoset , Polyester, TS , Silicone
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dielectric Polymers NT-5521-2 Photo Processing Tape  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film processing. Tape offers ease of use in dispensers and clean removal to eliminate leader card clean up.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Adhesive
50.8 microns
2.00 mil
Backing
Mechanical Properties Metric English Comments
Elongation at Break 90 %
90 %
Peel Strength 0.38347 kN/m
2.1875 pli
Adhesion
8.77 kN/m
50.0 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
>= 260 °C
>= 500 °F
Shear Adhesive Failure (polyester failure)
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Yellow
Users viewing this material also viewed the following: