Dielectric Polymers NT-2802SW Functional Splice Tape  (discontinued **)

Category Polymer , Adhesive , Tape , Thermoset , Polyester, TS , Silicone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dielectric Polymers NT-2802SW Functional Splice Tape  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crosslinked silicone adhesive with silicone easy release coated polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of roll label stock and substrates to be coated with a pressure sensitive adhesive. The silicone easy release coating on the back side of the PET creates a functional splice, making it ideal for sequential label applications. Also used to cover idlers and other in-process rolls that come in contact with pressure sensitive adhesives.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Backing
50.8 microns
2.00 mil
Adhesive
Mechanical Properties Metric English Comments
Elongation at Break 130 %
130 %
Peel Strength 0.438 kN/m
2.50 pli
Adhesion
6.14 kN/m
35.0 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
>= 260 °C
>= 500 °F
Shear Adhesive Failure (polyester failure)
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Burgundy