Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Softflex® SF 5596 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® SF 5596 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
ASTM D2240
Tensile Strength at Break 3.30 MPa
479 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 600 %
600 %
chs 2.0 in/min; ASTM D638
Tear Strength 28.0 kN/m
160 pli
ASTM D624
Copyright © lookpolymers.com All Rights Reserved