Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Melt Flow 37 g/10 min

@Load 2.16 kg,
Temperature 190 °C
37 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 50
40 - 50
ASTM D2240
Tensile Strength, Yield 4.10 MPa
595 psi
chs 20 in/min; ASTM D638
Elongation at Break 750 %
750 %
chs 20 in/min; ASTM D638
Tear Strength 24.5 kN/m
140 pli
ASTM D624