Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.25 %

@Temperature 23.0 °C,
Time 86400 sec
0.25 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Melt Flow 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Yield 62.0 MPa
8990 psi
chs 2.0 in/min; ASTM D638
Flexural Strength 85.0 MPa
12300 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm
16.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
0.125";; ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified