Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers PC 1001 GF30 30% Glass Reinforced Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers PC 1001 GF30 30% Glass Reinforced Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 124 MPa
18000 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 6.897 GPa
1000 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved