Diamond Polymers PC 0814 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers PC 0814 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.277 GPa
330.3 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
0.125";; ASTM D648