Diamond Polymers NYLON 66GF33 Black

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NYLON 66GF33 Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
flow direction; ASTM D955
0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
transverse direction; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength at Break 199.8 MPa
28980 psi
ASTM D638
Elongation at Break 24 %
24 %
ASTM D638
Flexural Strength 282.5 MPa
40970 psi
ASTM D790
Flexural Modulus 9.301 GPa
1349 ksi
ASTM D790
Izod Impact, Notched 1.175 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.201 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Tensile Impact Strength 126.2 kJ/m²
60.05 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
0.125";; ASTM D648