Diamond Polymers NYLON 6615 Black, Super Tough

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NYLON 6615 Black, Super Tough.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 50 - 60 %
50 - 60 %
ASTM D638
Flexural Strength 61.0 MPa
8850 psi
ASTM D790
Flexural Modulus 1.655 GPa
240.0 ksi
ASTM D790
Izod Impact, Notched 8.00 - 9.00 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 - 16.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
NB

@Thickness 3.17 mm,
Temperature -40.0 °C
NB

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 133 - 160 J/cm

@Thickness 3.17 mm
249 - 300 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648