Diamond Polymers NPP30-3500F Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP30-3500F Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
chs 50 mm/min; tangent; ASTM D638
Elongation at Yield 8.0 %
8.0 %
chs 50 mm/min; tangent; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm
0.401 ft-lb/in

@Thickness 0.125 in
ASTM D256