Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP30-2400 GF20 20% Glass Filled Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP30-2400 GF20 20% Glass Filled Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
chs 0.2 in/min; ASTM D638
Elongation at Yield 3.0 %
3.0 %
chs 0.2 in/min; ASTM D638
Flexural Modulus 3.541 GPa
513.6 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm

@Thickness 3.17 mm
1.69 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
0.125";; ASTM D648
Descriptive Properties Value Comments
Glass Content (%) 20
ASTM D2584
Copyright © lookpolymers.com All Rights Reserved