Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP25-0802 GF20 20% Glass Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 20% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-0802 GF20 20% Glass Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ash 18 - 22 %
18 - 22 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 4.7 %
4.7 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.963 GPa
429.7 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.335 J/cm

@Thickness 3.17 mm
2.501 ft-lb/in

@Thickness 0.125 in
ASTM D256