Diamond Polymers NPP11-0119 Linear Low Density Polyethylene with Antiblock

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP11-0119 Linear Low Density Polyethylene with Antiblock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.6 MPa

@Thickness 0.0254 mm
4000 psi

@Thickness 0.00100 in
Transverse to Flow; ASTM D882
34.4 MPa

@Thickness 0.0254 mm
4990 psi

@Thickness 0.00100 in
Direction of Flow; ASTM D882
Elongation at Break 550 %

@Thickness 0.0254 mm
550 %

@Thickness 0.00100 in
Direction of Flow; ASTM D882
600 %

@Thickness 0.0254 mm
600 %

@Thickness 0.00100 in
Transverse to Flow; ASTM D882
Dart Drop, Total Energy 140 J
103 ft-lb
F50; ASTM D1709
Tear Strength Test 400
400
g; Direction of Flow; ASTM D1922
750
750
g; Transverse to Flow; ASTM D1922
Optical Properties Metric English Comments
Haze 20 %
20 %
ASTM D1003
Gloss 50 %
50 %
45°; ASTM D2457