Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP10-0105 Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP10-0105 Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Vinyl Acetate Content 4.6 %
4.6 %
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.7 MPa
3580 psi
Transverse to Flow; ASTM D882
25.9 MPa
3760 psi
Direction of Flow; ASTM D882
Elongation at Break 180 %
180 %
Direction of Flow; ASTM D882
580 %
580 %
Transverse to Flow; ASTM D882
1% Secant Modulus 146 MPa
21200 psi
Direction of Flow; ASTM D882
168 MPa
24400 psi
Transverse to Flow; ASTM D882
Dart Drop, Total Energy 190 J
140 ft-lb
F50; ASTM D1790
Tear Strength Test 90
90
g; Transverse to Flow; ASTM D1922
200
200
g; Direction of Flow; ASTM D1922
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.4 %
6.4 %
ASTM D1003
Gloss 71 %
71 %
45°; ASTM D2457