Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP 60-1300 GF30 30% Glass Filled Polyester Alloy

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP 60-1300 GF30 30% Glass Filled Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Viscosity 1.20e+6 cP

@Load 5.00 kg,
Temperature 250 °C
1.20e+6 cP

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103.5 MPa
15010 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 6.486 GPa
940.7 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Descriptive Properties Value Comments
Glass Content (%) 28-32
ASTM D5630
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved