Diamond Polymers DIAMALOY 800 Polycarbonate/Polyester Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 800 Polycarbonate/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 10.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
10.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.1 MPa
7270 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 4.1 %
4.1 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.108 GPa
305.7 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 204 °C

@Load 1.00 kg,
Thickness 3.17 mm
399 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in