Diamond Polymers ASAPC 122954H

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASAPC 122954H.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 13 g/10 min

@Load 5.00 kg,
Temperature 265 °C
13 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.6 MPa
7190 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.067 GPa
299.8 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.01 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 146 °C

@Load 1.00 kg,
Thickness 3.17 mm
295 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in