Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASA TW18B3 ASA Weatherable Polymers Injection Molding Grade, Very High Heat

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA TW18B3 ASA Weatherable Polymers Injection Molding Grade, Very High Heat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Melt Flow 1.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.5 MPa
7470 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.625 GPa
380.7 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.750 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.41 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 131 °C

@Load 1.00 kg,
Thickness 3.17 mm
268 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525