Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASA M806 ASA Weatherable Polymers Direct Metallizable Grade, Medium Heat

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA M806 ASA Weatherable Polymers Direct Metallizable Grade, Medium Heat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 22 g/10 min

@Load 10.0 kg,
Temperature 240 °C
22 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.8 MPa
7510 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.377 GPa
344.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.530 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.992 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256