Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ABSPC 8020 Very High Impact

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ABSPC 8020 Very High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 58.6 MPa
8500 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.398 GPa
347.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 6.40 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C

@Load 1.00 kg
257 °F

@Load 2.20 lb
ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved