Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ABS TS15v04 Injection Molding Grade, ABS/PC Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ABS TS15v04 Injection Molding Grade, ABS/PC Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 265 °C
10 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
chs 2 in/min; ASTM D638
Elongation at Yield 3.0 %
3.0 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.205 GPa

@Thickness 3.17 mm
319.8 ksi

@Thickness 0.125 in
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C

@Load 1.00 kg
261 °F

@Load 2.20 lb
ASTM D1525
Users viewing this material also viewed the following: