Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ABS TS-12 Injection Molding Grade, Medium Heat

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ABS TS-12 Injection Molding Grade, Medium Heat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 21 g/10 min

@Load 5.00 kg,
Temperature 265 °C
21 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.4 MPa
6290 psi
chs 2 in/min; ASTM D638
Elongation at Yield 2.5 %
2.5 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.136 GPa

@Thickness 3.17 mm
309.8 ksi

@Thickness 0.125 in
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.87 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C

@Load 1.00 kg
230 °F

@Load 2.20 lb
ASTM D1525
Users viewing this material also viewed the following: