Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Denka VINYKON R5020 PVC, R grade for hard extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON R5020 PVC, R grade for hard extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.486 g/cc
0.05369 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.183 MPa
6118.1 psi
JIS-K-6740
Elongation at Break 95 %
95 %
JIS-K-6740
Flexural Strength 73.0 MPa
10600 psi
JIS-K-6740
Flexural Modulus 3.75 GPa
544 ksi
JIS-K-6740
Izod Impact, Notched 0.3924 J/cm

@Temperature -20.0 °C
0.7351 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
0.59841 J/cm

@Temperature 0.000 °C
1.1211 ft-lb/in

@Temperature 32.0 °F
JIS-K-6740
0.7848 J/cm

@Temperature 23.0 °C
1.470 ft-lb/in

@Temperature 73.4 °F
JIS-K-6740
Penetration 81
81
[°C], penetration temperature; JIS-K-6740
Thermal Properties Metric English Comments
Vicat Softening Point 93.0 °C
199 °F
JIS-K-6740
Descriptive Properties Value Comments
Thermostability, min, JIS-K-6723 90
Copyright © lookpolymers.com All Rights Reserved