Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Denka VINYKON M558070 PVC, M grade for soft injection molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON M558070 PVC, M grade for soft injection molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.398 g/cc
0.05051 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
JIS-K-6301
Tensile Strength at Break 15.696 MPa
2276.5 psi
JIS-K-6723
Elongation at Break 290 %
290 %
JIS-K-6723
100% Modulus 0.0067689 GPa
0.98176 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -36.0 °C
-32.8 °F
JIS-K-6723
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved