Daikin POLYFLON D-1E PTFE Dispersion

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Daikin Industries
Trade Name POLYFLON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Daikin POLYFLON D-1E PTFE Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYFLON PTFE aqueous dispersions are normally stabilized with non-ionic surfactants and contain 60% POLYFLON PTFE by weight.Processing Methods: Impregnation, casting, coating.Applications: Anti-stick coating, packings, cast film.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
at 25°C
Particle Size 0.20 - 0.40 µm
0.20 - 0.40 µm
pH 9.0 - 10
9.0 - 10
Viscosity 0.25 cP

@Temperature 25.0 °C
0.25 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
PTFE Component
Oxygen Index >= 95 %
>= 95 %
PTFE Component
Electrical Properties Metric English Comments
Dielectric Constant 1.9 - 2.1

@Frequency 1000 Hz
1.9 - 2.1

@Frequency 1000 Hz
PTFE Component; ASTM D150
1.9 - 2.1

@Frequency 1e+6 Hz
1.9 - 2.1

@Frequency 1e+6 Hz
PTFE Component; ASTM D150
Dissipation Factor 0.00010 - 0.00022
0.00010 - 0.00022
PTFE Component