Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TW341 (COND) Nylon 46 Heat Stabilized, Lubricated (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW341 (COND) Nylon 46 Heat Stabilized, Lubricated (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
(DAM); ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/-2
Elongation at Yield >= 55 %
>= 55 %
Nominal; ISO 527-1/-2
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
(DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
IEC 60093
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60243-1
Comparative Tracking Index 400 V
400 V
IEC 60112
Users viewing this material also viewed the following: