Material Notes:
50% Glass Reinforced, Heat Stabilized, Wear and Friction Modified
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
dry; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 225 MPa
32600 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
Tensile Modulus 16.0 GPa
2320 ksi
dry; ISO 527-1/-2
Izod Impact Resistance 1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
Charpy Impact, Notched 1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 290 °C
554 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
dry; ISO 75-1/-2