DSM Stanyl® TW275F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Lubricated + Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW275F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.6 %
2.6 %
50% RH / 23°C; Similar to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 205 MPa
29700 psi
ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/-2
Tensile Modulus 10.5 GPa
1520 ksi
ISO 527-1/-2
Flexural Modulus 9.00 GPa
1310 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
8.00 kJ/m²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
ISO 75-1/-2