Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TQ261F5 PA46-GF25

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TQ261F5 PA46-GF25.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% Glass Reinforced, Heat Stabilized
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
dry; ISO 1183
Moisture Absorption 2.60 %
2.60 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
Elongation at Break 1.8 %
1.8 %
dry; ISO 527-1/-2
Tensile Modulus 8.00 GPa
1160 ksi
dry; ISO 527-1/-2
Flexural Modulus 7.40 GPa
1070 ksi
dry; ISO 178
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
dry; ISO 75-1/-2
Users viewing this material also viewed the following: