Material Notes:
Thermal conductive material, Flame Retardant
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
dry; ISO 1183
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 MPa
7250 psi
dry; ISO 527-1/-2
Elongation at Break 0.60 %
0.60 %
dry; ISO 527-1/-2
Tensile Modulus 9.10 GPa
1320 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
Thermal Conductivity 2.10 W/m-K
14.6 BTU-in/hr-ft²-°F
through plane; ASTM E1461
14.0 W/m-K
97.2 BTU-in/hr-ft²-°F
in plane; ASTM E1461
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
dry; IEC 60695-11-10
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
dry; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
dry; IEC 60093