DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
(DAM); ISO 1183
Moisture Absorption at Equilibrium 1.1 %
1.1 %
Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
DAM; ISO 294-4
0.0070 cm/cm
0.0070 in/in
DAM; ISO 294-4
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min (DAM); ISO 11357-1/-3
UL RTI, Electrical 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL746B
140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact 110 °C

@Thickness 0.750 mm
230 °F

@Thickness 0.0295 in
UL746B
125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL746B
125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
Electrical Properties Metric English Comments
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Descriptive Properties Value Comments
Flame Retardant Yes
Flame Retarding Agent Yes
Heat stabilized or stable to heat Yes
Injection molding Yes
Lubricants Yes
Platable Yes
Release Agent Yes
With Fillers Yes