DSM Dyneema® SB115

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer DSM Engineering Plastics
Trade Name Dyneema®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Dyneema® SB115.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SB115 is an Ultra-High Molecular Weight Polyethylene fiber based composite laminate for low weight soft armor applications. A roll of product consists of two single layers of unidirectional sheet cross plied at 90 degrees to each other, consolidated with a rubber based matrix and covered with a protective elm. SB115 produced in the United Stated of America complies with the provisions of the United States Code (USC) Title 10, Subchapter V, § 2533a (The Berry Amendment). SB115 is subject to jurisdiction of the U.S. Department of Commerce, and is exported using Export Control (No Suggestions) Number (ECCN) 1C990. Restrictions may therefore apply to the export and re-export of this product.
Physical Properties Metric English Comments
Coating Weight 75.0 - 84.0 g/m²
46.9 - 52.5 lb/ream
Areal Density; DTM LP152
Descriptive Properties Value Comments
Visual Defects per roll <22
DTM LP156