DSM Arnitel® CM622 TPC-ES

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer DSM Engineering Plastics
Trade Name Arnitel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnitel® CM622 TPC-ES.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60 Shore D, Extrusion
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-1/-2
Elongation at Break 500 %
500 %
ISO 527-1/-2
Tensile Modulus 0.230 GPa
33.4 ksi
ISO 527-1/-2
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 208 °C
406 °F
10°C/min; ISO 11357-1/-3
Vicat Softening Point 87.0 °C
189 °F
50 °C/h 50N; ISO 306
190 °C
374 °F
50 °C/h 10N; ISO 306