DSM Arnite® TB6 260 PBT-GB30

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Bead Filled
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® TB6 260 PBT-GB30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ISO 527-1/-2
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/-2
Elongation at Yield 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 4.50 GPa
653 ksi
ISO 527-1/-2
Charpy Impact Unnotched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Users viewing this material also viewed the following: