Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnite® T06 206 T Impact Modified PBT (European Grade)  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® T06 206 T Impact Modified PBT (European Grade)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame retardant gradesEasy molding FR grades for connectorsToughened unfilled materials for durabilityHigh modulus, tight specification for critical auto componentsToughened reinforced resinsLow outgassing grades for reflector surfacesArnite extrusion resins: Specialized materials for specific usesPET for medical applicationsLoose buffer Optical fiber tubingPET for stock shapesApplicationsAutomotive:Connectors, sensors and E&E parts, Exterior fittings, Gear housings and motors, Brake valve bodiesElectrical & Electronic: Telecoms and IT connectors, Bobbins, Low voltage Power distribution, E-motor components, Lightings and Lamp fittingsConsumer Durables: Small AppliancesOther: Optical fiber tubingInformation provided by DSM.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-1/-2
Elongation at Break 40 %
40 %
ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Descriptive Properties Value Comments
High impact or impact modified Yes
Injection molding Yes
Release Agent Yes
Without Fillers Yes
Users viewing this material also viewed the following: