DSM Arnite® AV2 390 XT PET GF50

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® AV2 390 XT PET GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% Glass Reinforced, Applications with extremely narrow tolerances
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
Sim. To ISO 62
Moisture Absorption 0.120 %
0.120 %
Sim. To ISO 62
Viscosity 15000 cP

@Shear Rate 100000 1/s,
Temperature 315 °C
15000 cP

@Shear Rate 100000 1/s,
Temperature 599 °F
20000 cP

@Shear Rate 100000 1/s,
Temperature 295 °C
20000 cP

@Shear Rate 100000 1/s,
Temperature 563 °F
25000 cP

@Shear Rate 100000 1/s,
Temperature 270 °C
25000 cP

@Shear Rate 100000 1/s,
Temperature 518 °F
200000 cP

@Shear Rate 1000 1/s,
Temperature 295 °C
200000 cP

@Shear Rate 1000 1/s,
Temperature 563 °F
230000 cP

@Shear Rate 1000 1/s,
Temperature 315 °C
230000 cP

@Shear Rate 1000 1/s,
Temperature 599 °F
300000 cP

@Shear Rate 1000 1/s,
Temperature 270 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 518 °F
Linear Mold Shrinkage, Flow 0.0045 cm/cm
0.0045 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 210 MPa
30500 psi
ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 19.0 GPa
2760 ksi
ISO 527-1/-2
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
6.50 J/cm²

@Temperature -30.0 °C
30.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
IEC 60695-11-10
HB

@Thickness 0.810 mm
HB

@Thickness 0.0319 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
IEC 60250
3.8

@Frequency 100 Hz
3.8

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
IEC 60250
0.011

@Frequency 1.00e+6 Hz
0.011

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112