Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
(DAM); ISO 1183
Water Absorption 9.0 %
9.0 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 2.5 %
2.5 %
Humidity Absorption (DAM); Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 22 %
22 %
ISO 527-1/-2
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-1/-2
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min (DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
IEC 60250
8.0

@Frequency 100 Hz
8.0

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1
Dissipation Factor 0.080

@Frequency 1e+6 Hz
0.080

@Frequency 1e+6 Hz
IEC 60250
0.125

@Frequency 100 Hz
0.125

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Flame Retardant Yes
Flame Retarding Agent Yes
Heat stabilized or stable to heat Yes
Injection molding Yes
Release Agent Yes
Without Fillers Yes