Material Notes:
25% Glass Reinforced, Flame Retardant (Halogen free), Heat Stabilized
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
dry; ISO 1183
Water Absorption 6.1 %
6.1 %
Sim. To ISO 62
Moisture Absorption 1.60 %
1.60 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 85.0 MPa
12300 psi
dry; ISO 527-1/-2
Elongation at Break 4.8 %
4.8 %
dry; ISO 527-1/-2
Tensile Modulus 6.50 GPa
943 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
dry; IEC 60695-11-10
V-2

@Thickness 0.800 mm
V-2

@Thickness 0.0315 in
dry; IEC 60695-11-10
Glow Wire Test 960 °C

@Thickness 1.60 mm
1760 °F

@Thickness 0.0630 in
Glow Wire Flammability Index, dry; IEC 60695-2-12
960 °C

@Thickness 0.750 mm
1760 °F

@Thickness 0.0295 in
Glow Wire Flammability Index, dry; IEC 60695-2-12