DP7-3003 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DP7-3003 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength, Ultimate 25.61 MPa
3714 psi
ASTM D412
Tensile Strength, Yield 7.233 MPa
1049 psi
at 100%; ASTM D412
Elongation at Break 458 %
458 %
ASTM D412
Tear Strength 98.9 kN/m
564 pli
die B; ASTM D624