Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DIAB TBR® 10 Multifunctional Polymer Core Material

Category Other Engineering Material , Composite Core Material , Polymer , Renewable/Recycled Polymer
Manufacturer DIAB Inc.
Trade Name TBR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DIAB TBR® 10 Multifunctional Polymer Core Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TBR® is a multifunctional polymer core designed for hard points within sandwich structures where through-bolting or point-loading would normally cause local crushing of low density sandwich cores. TBR® provides strength and performance for applications where there is a need for hard points and through bolting while maintaining lightweight construction. Typical applications include bolt transoms (outboard and inboard/outboard), deck cleat and railing bases winch pads, strut bases, and thru-hull pads. TBR® is available in three densities as standard sheets or fabricated kits. TBR® may contain up to 10% recycled content. It has a highly imidized chemical structure within its inter-penetrating polymer network. TBR® has a coarse cell structure designed for increased mechanical adhesion.Information provided by DIAB, Inc.
Physical Properties Metric English Comments
Density 0.160 g/cc
0.00579 lb/in³
Nominal
0.144 - 0.192 g/cc
0.00521 - 0.00694 lb/in³
Range represents a tolerance from nominal of -10%/+20%; ASTM D1622
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.10 MPa
740 psi
ASTM D1623
Elongation at Break 11.5 %
11.5 %
Shear Strain; ASTM C273
Compressive Strength 3.45 MPa
500 psi
ASTM D1621
Compressive Modulus 0.228 GPa
33.0 ksi
ASTM D1621-B
Poissons Ratio 0.32
0.32
Shear Modulus 0.0579 GPa
8.40 ksi
ASTM C273
Shear Strength 2.41 MPa
350 psi
ASTM C273
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 82.2 °C
180 °F
Continuous
Minimum Service Temperature, Air -198.3 °C
-324.9 °F
Continuous
Processing Properties Metric English Comments
Processing Temperature <= 90.0 °C
<= 194 °F
Descriptive Properties Value Comments
Water Absorption 0.005 lb/ft²
ASTM D2842 at 72°F