Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DIAB Divilette® 650 HV Polyester Resin-based Core Bedding Adhesive

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer DIAB Inc.
Trade Name Divilette®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DIAB Divilette® 650 HV Polyester Resin-based Core Bedding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Divilette is a polyester resin based core bedding adhesive specifically formulated for use with Diab's structural core materials. It is catalyzed with standard MEKP catalyst. Proper use of Divilette ensures all of the cuts in the core are completely filled and that no air entrapment exists between the core and the laminate. It is easy to apply with no run on vertical surfaces. Divilette can be applied with a spray applicator or hand towel.Divilette must be catalyzed with an MEKP 9% active oxygen content catalyst.Divilette exhibits less than a 1% linear shrinkage (ASTM D2566).Information provided by DIAB, Inc.
Physical Properties Metric English Comments
Density 0.650 g/cc
0.0235 lb/in³
Viscosity 100000 - 120000 cP

@Temperature 22.2 °C
100000 - 120000 cP

@Temperature 72.0 °F
ASTM D1824
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 1.00 GPa
145 ksi
ASTM D638
Thermal Properties Metric English Comments
Shrinkage <= 1.0 %
<= 1.0 %
ASTM D2566
Processing Properties Metric English Comments
Gel Time 30.0 - 45.0 min
30.0 - 45.0 min
ASTM D2471
Descriptive Properties Value Comments
Water Absorption 80 oz
Copyright © lookpolymers.com All Rights Reserved